Fig. 5From: Freeze-thaw durability of repair mortars and porous limestone: compatibility issuesFrost damage of cubic mortar specimens: a scaling (K50 after 5 freeze-thaw cycles) and b rounding of edges, surface scaling, and cracking (K50 after 11 freeze-thaw cycles) (red arrows show scaling, while white arrows point to microcracks)Back to article page